有關電鍍問題,有請相關專家解惑

  有個已經衝床過的鋁製製品,要整支陽極電鍍但是希望背面上下兩側要有20mm的長不能有電鍍,目前已知可以再電鍍之前貼上膠帶來防止電鍍,但是電鍍交代都奈不住電鍍都會電過去(電鍍老闆說至少電鍍5條以上,真的超硬),請問有什麼辦法可以解決?
  現在手上有約2000上下的東西,老闆說現在要用磨的但是我看會磨到死...,請他送雷射雕刻說太貴、車床又說不要,總之就是要免費就是,直說買台沙布機來來磨,結果磨超過5條東西又報銷不良...,請問還有什麼辦法?現在心想心一橫全磨了但是日後還需解決。

  請推薦我電鍍膠帶,或請教全部電鍍可以快速磨掉又不傷太多鋁件的方法!!

雷射雕窟-太貴
車床-有車道橫、價格稍貴
洗氫氧化鈉-有毒、不好控制
電鍍膠帶-問過幾家沒辦法給我浸泡時間只能說給我試用品試試....

= = = = = 8/1新增= = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = =
  聽到師傅說老闆的預算兩邊2cm加起來2塊錢也在嫌貴!!說我別白費工夫了,我想還是提出個改進方案出來,來證明他的方法錯的離譜!
  說什麼效率太差星期六加班算懲罰?巧婦難為無米之炊阿...

= = = = = 8/4新增= = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = =
家裡出了點事現在才來更新討教...

基本上物品狀態是這樣,有六種板子長度一樣寬度略為不同有20mm、30mm、40mm全部陽極電鍍,如圖片上下統一要有20mm要裸露鋁板要導電希望不要電鍍,上下兩側都有沖孔要裝螺絲
有關電鍍問題,有請相關專家解惑

請教各路前輩還有什麼方法把那兩側"快速""便宜"把它用掉?

小抱怨,星期五又撐到12點,工業這一行有沒有這麼趕?說要東西出貨就是要出貨?有問題的物件經過新修改連試都沒試過修一修就出去了,這真的是專業?

這不變成把客人當qc了?
= = = = = 8/10新增= = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = = =
該放炮慶祝了,測試了結果三隻有一隻被滲透,剩下兩隻會有收縮約1mm挺可惜的

膠帶材質問題?感覺像複合材料....
2013-07-30 22:38 發佈
文章關鍵字 電鍍問題 專家
我公司電鍍部門有用一種銀色的膠帶

黏性非常強,有點厚度

你找一下鐵氟龍膠帶


kenny877bal wrote:
我公司電鍍部門有用一...(恕刪)


鐵氟龍膠帶?鐵氟龍材質不是耐磨用的嗎?
曾經看過...把不要陽極處理的地方用網版印刷遮住,陽極後再把油墨洗掉~~~
請問是要陽極 還是電鍍
陽極後應該尺寸會減少吧
電鍍看要是鍍鎳或是其它 那個才會變厚

花錢請人用吧
全部電鍍後做一個治具蓋上去
可以露出約5條的高度
用人家做模具 那種可以磁鐵吸住和來回磨的機器磨掉(我忘了怎么稱呼)

不想花錢就當藝術品做吧!
不過手工要精準到磨掉五條.......

mick00614 wrote:
鐵氟龍膠帶?鐵氟龍材...(恕刪)


剛剛打去工廠問,說是地球牌的膠帶(表面灰色)

副廠長說以前試過很多家都不能用,只有這家的可以

給你做參考~
mick00614 wrote:
  有個已...(恕刪)


錫箔膠帶可用,黏性夠強~
不然就用電鍍膠帶,外面再包覆工業用保潔膜(但包覆完包膜後,包膜封口還要再纏上1圈電鍍膠帶避免包膜脫落)~
這樣就不會脫落,我們公司鍍厚20條~30條都是這樣處理(硬鉻)

白色黑狗 wrote:
曾經看過...把不要...(恕刪)


out!說成本太高@$#$%$%^

再說也要印刷、烘烤那時間要是能用膠帶來貼.......

我不是兇手 wrote:
錫箔膠帶可用,黏性夠...(恕刪)


沒辦法包覆,因為有一面要裸露,只有單面局部不要電鍍...

kenny877bal wrote:
剛剛打去工廠問,說是...(恕刪)


這有意思,現在就是不知道「電鍍」、「電鍍陽極」能不能用?最主要是要耐酸鹼經過4小時多的浸泡....